Calendar ageing
Calendar ageing is the permanent capacity a lithium battery loses with the passage of time, whether or not it is used. It is worst at high state of charge and high temperature.
Key facts
- •It is separate from cycle ageing, and the two run together
- •It is driven by slow growth of the passivating film on the anode, which consumes lithium
- •A full pack in a hot warehouse can lose 10–15 per cent of its capacity in a year
- •Storing at 40–60 per cent charge in the coolest available place slows it
- •As a rule of thumb, reaction rates roughly double for each 10 °C rise
How it works
At high state of charge the anode sits at the potential most favourable to electrolyte decomposition. The protective film formed during manufacture keeps growing slowly, and the lithium consumed by that growth never returns. Lower the charge and the reaction slows. Lower the temperature and it slows again.
This is not the same as self-discharge. Charge lost to self-discharge can be put back by recharging. Capacity lost to calendar ageing cannot.
A worked example
Take an illustrative ₹60,000 pack of 5.12 kWh that loses 12 per cent of its capacity during a year of hot, fully charged storage. It now holds about 4.51 kWh. If its value tracks capacity, ₹7,200 has gone. Twelve per cent interest on the same stock would also cost ₹7,200, so the ageing has doubled the true holding cost, and nothing on the stock sheet shows it.
The numbers are illustrative and real rates vary with cell and conditions. The point is the comparison: for batteries, holding cost is more than the cost of working capital.
Why it matters in India
High ambient temperature makes this a larger cost here than a temperate-climate data sheet implies. It matters to anyone holding stock: distributors, vehicle makers with buffer inventory, and financiers holding repossessed fleets. It also matters to backup systems, which sit full for long periods and may therefore age more through time than through use.
- •Store part-charged, not full, if stock will sit for months
- •Avoid metal-roofed stores and rooms that also hold chargers
- •Rotate stock first-in-first-out, and record arrival date and storage charge
- •Capacity-test a sample before shipping aged stock
Common mistakes
- •Assuming a new-looking, unused pack has its full rated capacity
- •Modelling only cycle-based degradation in a low-use application
- •Using a warranty term from a cooler market without adjusting for ambient temperature
Frequently asked questions
Does a battery age if it is never used?+
Yes. Chemical ageing continues in storage, which is why a pack that has sat for eighteen months is not equal to a newly made one, even with no recorded cycles. Its condition depends on how warm it was kept and at what charge.
How can you tell how much capacity a stored battery has lost?+
Run a capacity test: charge it fully, discharge it at a stated current to the cut-off voltage, and count the energy delivered. For large stock, test a representative sample from each batch, since the label and the appearance of a pack say nothing about this.
Read more
Related terms
Want this applied to your own numbers?
Every solution page carries a calculator that shows its own arithmetic — storage savings, lithium against lead-acid, and home pack sizing.